Baseline
What the customer was running
- Six-shoe table running at 1700 RPM
- Feed size of 1" × 2"
- Output size of 1/4" minus
- OEM standard chrome shoes — 24 hours run time per set
Parts
Si-Tec® ceramic shoes on the bench after 72 hours in a VSI, wear face up. Close enough that the ceramic reinforcement in the wear zone reads.
Measured on site
Wear life for the shoes improved by 200%, going from 24 hours to 72 hours.
Cemco 80 VSI crusher — one machine, one feed material
The record
The improvement only means something against what the machine was doing before it. Published 22 January 2020.
What the customer was running
What the change was meant to do
What was measured
What it was worth to the operation
Read this too
A wear part that lasts twice as long in Tennessee sandstone can do nothing of the kind in Idaho RAP, because the rock, the tonnage, and the geometry are different. Nothing here is a warranty and nothing here is a specification. What SI will do is measure your part in your circuit and put the numbers against the ones you have now.
How Si-Tec® is specifiedService life in hours or tons, the feed material, and photographs of where the wear actually is. That is enough to say whether Si-Tec® changes anything in your circuit.